Addition of endothermic fire retardants to provide near neutral pH pulp fiber webs
US8663427B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 7, 2011 |
| Grant date | Mar 4, 2014 |
| Priority date | — |
| Expiry date | Jul 19, 2031 |
Classification
- Technology area (CPC D)Textiles; Paper
- CPC primaryD21H21/24
- WIPO fieldTextile and paper machines
- WIPO sectorMechanical engineering
Abstract
A process in which an at least partially delignified pulp fiber web having a Kappa number of less than about 130 is treated with an aqueous endothermic fire retardant solution having a pH of about 10 or less. The treated pulp fiber web has a near neutral pH of from about 5 to about 9, and is treated with at least about 20 lbs of endothermic fire retardants per ton of the pulp fiber web, with at least about 5% of the total amount of endothermic fire retardants being added at a point prior to when the pulp fiber web is formed. Also a fire resistant pulp fiber web having a near neutral pH.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.