Abstract

A method for preparing pimaric acid type resin acids includes the following steps: step (1) adding refined resin acid, turpentine, or rosin along with maleic anhydride at a mass ratio of 1:0.3-1.5 into a reaction bottle, dissolving the ingredients into a C1-C10 lower fatty acid solvent, the mass ratio of the C1-C10 low fatty acid to refined resin acid is 0.05-30:1, then carrying out additional reaction by heating directly or with assistance of a microwave, subsequently cooling, crystallizing, filtering, and washing; and step (2) combining the filtrates collected in step (1), stripping the solvent by vacuum distillation to obtain pimaric acid type resin acid coarse product, dissolving the resulting coarse product in NaOH aqueous solution to prepare aqueous solution of pimaric acid type resin acid salt, adjusting the pH level to 6-14 with a mineral acid or an organic acid while stirring, and either directly purifying or acidifying followed by purifying, the resulting precipitation to obtain the final product. The method has the characteristics of high yield, high product content, low cost, and low environmental pollution.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.