Nonmagnetic high-hardness alloy

US8696836B2 · kind B2 · utility

5Cited by
9References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 2, 2006
Grant dateApr 15, 2014
Priority date
Expiry dateMay 2, 2028

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C19/058
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention provides a nonmagnetic high-hardness alloy having a Ni-based alloy composition containing; by weight %, C of 0.1% or less: Si of 2.0% or less; Mn of 2.0% or less; P of 0.03% or less; S of 0.01% or less; Cr of 30 to 45%; Al of 1.5 to 5.0%; and a balance of unavoidable impurities and Ni, the nonmagnetic high-hardness alloy being subjected to cold or warm plastic working and then ageing treatment, and a method for producing the nonmagnetic high-hardness alloy.