Patent · US Active

Nickel-base superalloy with improved degradation behavior

US8696980B2 · kind B2 · utility

1Cited by
6References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 3, 2011
Grant dateApr 15, 2014
Priority date
Expiry dateSep 14, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C19/057
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A nickel-base superalloy with improved degradation behavior consists essentially of the following chemical composition (details in % by weight): 7.7-8.3 Cr, 5.0-5.25 Co, 2.0-2.1 Mo, 7.8-8.3 W, 5.8-6.1 Ta, 4.9-5.1 Al, 1.3-1.4 Ti, 0.1-0.6 Pt, 0.1-0.5 Nb, 0.11-0.15 Si, 0.11-0.15 Hf, 200-750 ppm C, 50-400 ppm B, and the remainder Ni and production-related impurities.