Method for manufacturing a high alloy pipe

US8701455B2 · kind B2 · utility

1Cited by
4References
2Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 31, 2009
Grant dateApr 22, 2014
Priority date
Expiry dateMar 21, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/44
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for manufacturing a high alloy pipe comprises hot working, a high alloy material pipe having controlled amounts of C, Si, Mn, P, S, Ni, Cr, Mo, Cu, Al, N, O, and optionally Ca, Mg, and rare earth elements, with the balance Fe. The pipe composition satisfies the formula N×O≦0.001. The pipe is subjected to cold working to form the high alloy pipe, wherein the final cold working process is performed under the condition that a working ratio Rd in the reduction of area satisfies 15≦Rd (%)≦370×(C+N), where N, O and C are the contents (by mass percent) of the respective elements, and Rd is the working ratio (%) in the reduction of area. The pipe has an excellent ductility and an excellent corrosion resistance when cold working is performed to obtain a high strength after pipe-making.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.