Patent · US Active

Lead free dezincification alloy and method of making same

US8721765B2 · kind B2 · utility

0Cited by
5References
22Claims
0Family size

Assignee

Inventor

Key dates

Filing dateOct 24, 2012
Grant dateMay 13, 2014
Priority date
Expiry dateNov 16, 2032

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/08
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of producing a brass is disclosed. The alloy contains trace amounts of iron, manganese or aluminum. Phosphorous is added to a zinc, copper melt and combined with the iron, manganese and aluminum to form intermetallics. Additional phosphorous is added so the melt contains between about 0.08 to 0.15% phosphorous. A low lead brass alloy is provided. The alloy has tin in the range of 0.15% to 0.35%.