Patent · US Active

Chemical synthesis for graphene sheets greater than 1 μm in length

US8728578B2 · kind B2 · utility

0Cited by
0References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 12, 2011
Grant dateMay 20, 2014
Priority date
Expiry dateMay 12, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01B2204/32
  • WIPO fieldMicro-structural and nano-technology
  • WIPO sectorChemistry

Abstract

A method for preparing a graphene sheet greater than 1 μm in length that includes: combining graphitic oxide with a solvent having a ratio of from about 50:50 to about 80:20 deionized water and ethanol to form a graphitic oxide solution; mixing a solution of NaBH4 and deionized water and the graphitic oxide solution to form a mixture having a concentration of from 10 mmolar to 20 mmolar NaBH4; depositing the mixture on a substrate to form a sheet; and heating the mixture at a temperature of from 25° C. to 85° C. for from 3 to 30 minutes.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.