Lithium-titanium complex oxide and manufacturing method thereof, and battery electrode using same
US8741172B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Nov 28, 2012 |
| Grant date | Jun 3, 2014 |
| Priority date | — |
| Expiry date | Aug 4, 2033 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A lithium-titanium complex oxide whose total water generation amount and total carbon dioxide generation amount measured by thermal decomposition GC-MS are preferably 1500 wt ppm or less and 2000 wt ppm or less, respectively, is obtained by subjecting a mixture of titanium compound and lithium compound to a heat treatment at 600° C. or above, cooling the obtained reaction product to 50° C. or below, and then subjecting the cooled reaction product to a reheat treatment involving heating to the maximum temperature of 300 to 700° C. and then cooling, wherein the dew point of the ambience of the reheat treatment is controlled at −30° C. or below at a temperature of 200° C. or above.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.