Patent · US Active

Ni-based single crystal superalloy

US8771440B2 · kind B2 · utility

4Cited by
6References
11Claims
0Family size

Assignees

Inventors

Key dates

Filing dateSep 12, 2007
Grant dateJul 8, 2014
Priority date
Expiry dateApr 21, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A Ni-based single crystal superalloy according to the invention has, for example, a composition including: 5.0 to 7.0 wt % of Al, 4.0 to 10.0 wt % of Ta, 1.1 to 4.5 wt % of Mo, 4.0 to 10.0 wt % of W, 3.1 to 8.0 wt % of Re, 0.0 to 2.0 wt % of Hf, 2.5 to 8.5 wt % of Cr, 0.0 to 9.9 wt % of Co, 0.0 to 4.0 wt % of Nb, and 1.0 to 14.0 wt % of Ru in terms of weight ratio; and the remainder including Ni and incidental impurities. In addition, the contents of Cr, Hf and Al are preferably set so as to satisfy the equation OP≧108. According to the Ni-based single crystal superalloy of the invention, high creep strength can be maintained and the oxidation resistance can be improved.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.