Dispersion, slurry and process for producing a casting mould for precision casting using the slurry
US8778449B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Mar 30, 2010 |
| Grant date | Jul 15, 2014 |
| Priority date | — |
| Expiry date | Apr 21, 2031 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08K3/22
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Slurry which contains a) from (50) to (80)% by weight of refractory particles having an average particle size of from (0.5) m to (150) m, b) from (5) to (35)% by weight of aluminum oxide particles having an average particle diameter of less than (300) nm and c) from (5) to (35)% by weight of water and d) a pH of from (5) to (12). Process for producing the slurry using a dispersion, and also the dispersion itself. Process for producing a casting mold, and also the casting mold itself.