Method for producing a glass fiber and device
US8800324B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 17, 2010 |
| Grant date | Aug 12, 2014 |
| Priority date | — |
| Expiry date | Oct 24, 2030 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03B2205/56
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A method for producing a glass fiber, through longitudinally drawing a preform in a drawing kiln, wherein cooling the glass fiber is performed in at least three time periods, wherein the glass fiber is exposed to a first time based cooling rate above a crystallization temperature range, to a second time based cooling rate that is greater than the first time based cooling rate within the crystallization temperature range, and to a third time based cooling rate which is smaller than the second time based cooling rate below the crystallization temperature range.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.