Patent · US Active

Effect of wet reduction on catalyst stability and methods of maintaining catalyst stability

US8802912B2 · kind B2 · utility

0Cited by
23References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 23, 2009
Grant dateAug 12, 2014
Priority date
Expiry dateNov 26, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC10G2300/703
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

The present invention provides a method of increasing stability of a catalyst used in a dehydrogenation process. The method includes storing fresh catalyst in a reduction zone, passing a gas through the reduction zone, introducing hydrocarbons and hydrogen gas into a reactor positioned downstream from the reduction zone to facilitate a dehydrogenation reaction, and replenishing spent catalyst in the reactor with fresh catalyst from the reduction zone. The gas has a moisture content at or below about 4000 ppmv and a temperature at or below about 290° C. The reactor includes catalyst for increasing the rate of the dehydrogenation reaction. The moisture content of the gas may be reduced to at or below about 4000 ppmv by passing the gas through a drier or by using an inert gas stream. The temperature of the gas may also be reduced.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.