Spark plug including electrodes with low swelling rate and high corrosion resistance

US8816577B2 · kind B2 · utility

2Cited by
8References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 14, 2012
Grant dateAug 26, 2014
Priority date
Expiry dateOct 20, 2032

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01T21/02
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A spark plug (20) includes a center electrode (24) and a ground electrode (22). The electrodes (22, 24) include a core (26) formed of a copper (Cu) alloy and a clad (28) formed of a nickel (Ni) alloy enrobing the core (26). The Cu alloy includes Cu in an amount of at least 98.5 weight percent, and at least one of Zr and Cr in an amount of at least 0.05 weight percent. The Cu alloy includes a matrix of the Cu and precipitates of the Zr and Cu dispersed in the Cu matrix. The Ni alloy of the clad (28) includes Ni in an amount of at least 90.0 weight percent. The Ni alloy also includes at least one of a Group 3 element, a Group 4 element, a Group 13 element, chromium (Cr), silicon (Si), and manganese (Mn) in a total amount sufficient to affect the strength of the Ni alloy.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.