Patent · US Active

Hot stretch straightening of high strength age hardened metallic form and straightened age hardened metallic form

US8834653B2 · kind B2 · utility

16Cited by
139References
15Claims
0Family size

Assignee

Inventor

Key dates

Filing dateJul 2, 2013
Grant dateSep 16, 2014
Priority date
Expiry dateSep 21, 2033

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12299
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for straightening an age hardened metallic form includes heating an age hardened metallic form comprising one of a titanium alloy, a nickel alloy, an aluminum alloy, and a ferrous alloy to a straightening temperature of at least 25° F. below the age hardening temperature, and applying an elongation tensile stress for a time sufficient to elongate and straighten the form. The elongation tensile stress is at least 20% of the yield stress and not equal to or greater than the yield stress at the straightening temperature. The straightened form deviates from straight by no greater than 0.125 inch over any 5 foot length or shorter length. The straightened form is cooled while simultaneously applying a cooling tensile stress that balances the thermal cooling stress in the metallic form to thereby maintain a deviation from straight of no greater than 0.125 inch over any 5 foot length or shorter length.