Abstract

Provided is an Ni-base alloy excellent in strength, ductility and other properties through the resolution of micro-segregation. Also provided is a process for manufacturing an Ni-base alloy containing by mass C:0.15% or less, Si:1% or less, Mn:1% or less, Cr:10 to 24%, Mo+(1/2)W (where Mo may be contained either alone or as an essential component):5 to 17%, Al:0.5 to 1.8%, Ti:1 to 2.5%, Mg:0.02% or less, and either B:0.02% or less and/or Zr:0.2% or less at an Al/(Al+0.56Ti) ratio of 0.45 to 0.70 with the balance consisting of Ni and impurities, which comprises subjecting, at least one time, an Ni-base alloy material which is prepared by vacuum melting and has the above composition to homogenization heat treatment at 1160 to 1220° C. for 1 to 100 hours. The Mo segregation ratio of the alloy is controlled to 1 to 1.17 by the homogenization heat treatment.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.