Patent · US Active

Steel alloy for a low-alloy steel for producing high-strength seamless steel tubing

US8865061B2 · kind B2 · utility

1Cited by
0References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 23, 2009
Grant dateOct 21, 2014
Priority date
Expiry dateMay 16, 2029

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/22
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The invention relates to a steel alloy for a low alloy steel for producing high-tensile, weldable, hot-rolled seamless steel tubing, in particular construction tubing. The chemical composition (in % by mass) is: 0.15-0.18% C; 0.20-0.40% Si; 1.40-1.60% Mn; max. 0.05% P; max. 0.01% S; >0.50-0.90% Cr; >0.50-0.80% Mo; >0.10-0.15% V; 0.60-1.00% W; 0.0130-0.0220% N; the remainder is made up of iron with production-related impurities; with the optional addition of one or more elements selected from Al, Ni, Nb, Ti, with the proviso that the relationship V/N has a value of between 4 and 12 and the Ni content of the steel is not more than 0.40%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.