Metal nanobelt and method of manufacturing the same, and conductive ink composition and conductive film comprising the same

US8865251B2 · kind B2 · utility

1Cited by
1References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 10, 2009
Grant dateOct 21, 2014
Priority date
Expiry dateDec 15, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12229
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention relates to a metal nanobelt and a method of manufacturing the same, and a conductive ink composition and a conductive film including the same. The metal nanobelt can be easily manufactured at a normal temperature and pressure without requiring the application of high temperature and pressure, and also can be used to form a conductive film or conductive pattern that exhibits excellent conductivity if the conductive ink composition including the same is printed onto a substrate before a heat treatment or a drying process is carried out at low temperature. Therefore, the metal nanobelt and the conductive ink composition may be applied very appropriately for the formation of conductive patterns or conductive films for semiconductor devices, displays, solar cells in environments requiring low temperature heating. The metal nanobelt has a length of 500 nm or more, a length/width ratio of 10 or more, and a width/thickness ratio of 3 or more.