Core shell phosphor and method of making the same

US8865305B2 · kind B2 · utility

0Cited by
6References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 16, 2010
Grant dateOct 21, 2014
Priority date
Expiry dateOct 20, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2989
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A method of making a core-shell phosphor is provided. The method comprises mixing a lanthanum phosphate (LaPO4) core with a shell precursor mixture comprising at least one compound of La, at least one compound of Ce, and at least one compound of Tb to form a core+shell precursor mixture, heating the core+shell precursor mixture to a temperature in a range from about 900° C. to about 1200° C. with an inorganic flux material in presence of a reductant to provide a heated core+shell precursor mixture, cooling the heated core+shell precursor mixture to ambient temperature to provide a product core-shell phosphor dispersed in the inorganic flux material; and separating the product core-shell phosphor from the inorganic flux material.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.