Patent · US Active

Ni-added steel plate and method of manufacturing the same

US8882942B2 · kind B2 · utility

2Cited by
1References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 7, 2011
Grant dateNov 11, 2014
Priority date
Expiry dateJul 7, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/001
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A Ni-added steel plate contains, by mass %, C: 0.03% to 0.10%, Si: 0.02% to 0.40%, Mn: 0.3% to 1.2%, Ni: 5.0% to 7.5%, Cr: 0.4% to 1.5%, Mo: 0.02% to 0.4%, Al: 0.01% to 0.08%, T.O: 0.0001% to 0.0050%, P: limited to 0.0100% or less, S: limited to 0.0035% or less, and N: limited to 0.0070% or less with a remainder composed of Fe and inevitable impurities, in which a Ni segregation ratio at a position of ¼ of a plate thickness away from a plate surface in a thickness direction is 1.3 or less, a fraction of austenite after deep cooling is 2% or more, an austenite unevenness index after deep cooling is 5.0 or less, and an average equivalent circle diameter of austenite after deep cooling is 1 μm or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.