Patent · US Active

Honeycomb structure and manufacturing method thereof

US8894915B2 · kind B2 · utility

1Cited by
10References
6Claims
0Family size

Assignee

Inventor

Key dates

Filing dateAug 21, 2008
Grant dateNov 25, 2014
Priority date
Expiry dateOct 21, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/24149
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A honeycomb structure is made of cordierite and has a plurality of cells separated from each other by porous partition walls and functioning as fluid passages. The honeycomb structure has a thermal expansion coefficient of 0.25×10−6/° C. or less, an average pore diameter is 3 to 8 μm, and a porosity of 25% or more. The honeycomb structure is made of cordierite excellent in thermal shock resistance even with large pore diameters and high porosity.