Preparation of industrial asphalt
US8901211B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 23, 2012 |
| Grant date | Dec 2, 2014 |
| Priority date | — |
| Expiry date | Sep 12, 2032 |
Classification
- Technology area (CPC E)Fixed Constructions
- CPC primaryE04D1/20
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention relates to a method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to about 12 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm to produce the industrial asphalt. The highly saturated rubbery polymer can be a styrene-ethylene/butylene-styrene block copolymer rubber or a highly saturated styrene-ethylene/propylene-styrene block copolymer rubber.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.