Polyurethane urea elastic fiber
US8920922B2 · kind B2 · utility
0Cited by
3References
7Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 3, 2007 |
| Grant date | Dec 30, 2014 |
| Priority date | — |
| Expiry date | Oct 16, 2028 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T442/413
- WIPO fieldTextile and paper machines
- WIPO sectorMechanical engineering
Abstract
Disclosed is a polyurethane urea elastic fiber containing 5-40% by weight of a polyurethane compound, wherein the compression deformation starting temperature determined by thermomechanical analysis (TMA) is not less than 150° C. but not more than 180° C. and time for thermal cutting at 180° C. is not less than 30 seconds.