Cellular elastomer with little tendency toward creep at high temperatures
US8927613B2 · kind B2 · utility
0Cited by
7References
18Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 14, 2009 |
| Grant date | Jan 6, 2015 |
| Priority date | — |
| Expiry date | Jul 14, 2029 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G18/7678
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention relates to cellular polyisocyanate polyaddition products whose density to DIN EN ISO 845 is from 200 to 800 kg/m3, and also to prepolymer composed of at least one diisocyanate (a) and of at least one polyether alcohol (b), where the at least one polyether alcohol (b) comprises the following components: