Heat adherent polyurethane film

US8927676B2 · kind B2 · utility

0Cited by
4References
2Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 20, 2008
Grant dateJan 6, 2015
Priority date
Expiry dateMay 21, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08J2375/08
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The object of the present invention is to provide a polyurethane film having heat adhesion and further having high stress retention and excellent elastic functions, and the polyurethane film of the present invention is a heat adherent polyurethane film wherein the thermal adhesion peeling stress indicated by a maximum stress when separating a film from a cotton fabric after hot-pressing the film to the cotton fabric at a temperature of 130° C. under a pressure of 4 bar for 25 seconds is 5.88 N/cm or more and the stress retention at an elongation percentage of 200% indicated by a ratio of a stress (fR) in recovery to a stress (fS) in stretching at an elongation percentage of 200% in an S-S curve drawn when the film is stretched to an elongation percentage of 300% and then recovered is 40% or more.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.