Spot welded joint

US8962149B2 · kind B2 · utility

4Cited by
0References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 30, 2010
Grant dateFeb 24, 2015
Priority date
Expiry dateNov 20, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12965
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

Provided is a spot welded joint (10) which includes at least one thin steel plate with a tensile strength of 750 MPa to 1850 MPa and a carbon equivalent Ceq of equal to or more than 0.22 mass % to 0.55 mass % and in which a nugget (3) is formed in an interface of the thin steel plates (1A, 1B). In a nugget outer layer zone, a microstructure consists of a dendrite structure in which an average value of arm intervals is equal to or less than 12 μm, an average grain diameter of carbides contained in the microstructure is 5 nm to 100 nm, and a number density of carbides is equal to or more than 2×106/mm2.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.