Method for preparation of high purity, crystalline cobalt nitrate from spent cobalt/silica catalyst
US8986644B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 5, 2014 |
| Grant date | Mar 24, 2015 |
| Priority date | — |
| Expiry date | Sep 5, 2034 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for preparing crystalline cobalt nitrate. The method includes: 1) calcining a spent Co/SiO2 catalyst, cooling the calcined material to room temperature, and grinding it to yield a powder; 2) heating the powder in a fluidized bed reactor; 3) adding the heated powder into excess dilute nitric acid solution and filtering to obtain a cobalt nitrate solution; 4) adjusting the pH value of the cobalt nitrate solution to 1.5, adding a preheated oxalic acid solution, adjusting a pH value of the resulting solution to 1.5, immediately filtering the resulting solution to yield a precipitate of cobalt oxalate, washing the precipitate of cobalt oxalate to yield a neutral filtrate; 5) drying the precipitate and calcining to yield cobalt oxide; 6) dissolving the cobalt oxide in nitric acid to yield a second cobalt nitrate solution; and 7) evaporating the second cobalt nitrate solution to obtain crystalline cobalt nitrate.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.