Patent · US Active

Hollow carbon microparticle and method for producing same

US8986838B2 · kind B2 · utility

2Cited by
5References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 11, 2009
Grant dateMar 24, 2015
Priority date
Expiry dateNov 22, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2993
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Elastic and ultra-lightweight hollow carbon fine particles and a method for producing such hollow carbon fine particles are to be provided. In the method, fine droplets are formed from a mixed solution containing a water soluble organic substance and lithium carbonate; composite fine particles of the water soluble organic substance and the lithium carbonate are prepared by drying the fine droplets formed from the mixed solution; and the composite fine particles are decomposed at a temperature in a range of 500° C. to 900° C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.