Patent · US Active

Method and composition for sequestration of arsenic

US8998790B2 · kind B2 · utility

7Cited by
4References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 4, 2013
Grant dateApr 7, 2015
Priority date
Expiry dateSep 4, 2033

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC03C3/087
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for sequestrating arsenic oxides, comprising forming an insoluble and stable glass incorporating a fully oxidized form of arsenic generated by oxidation of an initial lower oxide of arsenic and stabilization by calcium salt formation. The glass composition for sequestration of arsenic comprises from 50 to 75% silica; from 0.5 to 3% Al2O3; from 1 to 15% MnO; from 5 to 15% CaO; from 1 to 20% As2O5 and from 8 to 14% Na2O, less than four percent of iron oxides, magnesium oxide and other oxides.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.