Patent · US Active

Hydrostable polyetherimide blends, methods of manufacture, and articles formed therefrom

US9006319B2 · kind B2 · utility

3Cited by
18References
24Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 4, 2011
Grant dateApr 14, 2015
Priority date
Expiry dateMar 24, 2032

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08K5/49
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A composition comprising, based on the total weight of the composition, from 10 to 90 wt. % of a polyetherimide with a weight average molecular weight from 10,000 to 80,000 Daltons; from 10 to 90 wt. % of a polymer selected from polycarbonates, polyester-polycarbonates, polyalkylene terephthalates, or a combination thereof, from 0.005 to 1 wt. % of a hydrotalcite having a particle size of less than 10 micrometer and a magnesium oxide to aluminum oxide mole ratio of 1.0 to 5.0; from 0.01 to 1.0 wt. % of a phosphorus-containing stabilizer; from 0.01 to 1.00 wt. % of a hindered phenol stabilizer; optionally, from 0 to 3 wt. % of a polyolefin; and optionally, from 0 to 5 wt. % of an inorganic metal oxide.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.