Wet lamination process for reducing mud cracking in fuel cell components

US9012346B2 · kind B2 · utility

1Cited by
5References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 4, 2010
Grant dateApr 21, 2015
Priority date
Expiry dateJun 4, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/50
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

Methods of making a substantially crack-free electrode layer are described. The methods include depositing an electrode ink on a substrate; placing a solid polymer film on a surface of the wet electrode ink; drying the electrode ink; and removing the solid polymer film from the surface of the dry electrode ink to form the substantially crack-free electrode layer on the substrate.