Ionically-conductive amorphous lithium lanthanum zirconium oxide

US9034525B2 · kind B2 · utility

13Cited by
44References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 2, 2010
Grant dateMay 19, 2015
Priority date
Expiry dateJul 31, 2033

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/50
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Amorphous lithium lanthanum zirconium oxide (LLZO) is formed as an ionically-conductive electrolyte medium. The LLZO comprises by percentage of total number of atoms from about 0.1% to about 50% lithium, from about 0.1% to about 25% lanthanum, from about 0.1% to about 25% zirconium, from about 30% to about 70% oxygen and from 0.0% to about 25% carbon. At least one layer of amorphous LLZO may be formed through a sol-gel process wherein quantities of lanthanum methoxyethoxide, lithium butoxide and zirconium butoxide are dissolved in an alcohol-based solvent to form a mixture which is dispensed into a substantially planar configuration, transitioned through a gel phase, dried and cured to a substantially dry phase.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.