Hardened martensitic steel having a low or zero content of cobalt, method for producing a component from this steel, and component obtained in this manner
US9045806B2 · kind B2 · utility
3Cited by
6References
28Claims
0Family size
Assignee
Inventor
Key dates
| Filing date | Jun 18, 2008 |
| Grant date | Jun 2, 2015 |
| Priority date | — |
| Expiry date | Oct 16, 2030 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D1/58
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Steel, characterized in that the composition thereof is, in percentages by weight: Method of producing a component from this steel and a component obtained in this manner.