Method for producing hot rolled hollow sections having a rectangular cross-section and small edge radii
US9056344B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Aug 12, 2010 |
| Grant date | Jun 16, 2015 |
| Priority date | — |
| Expiry date | Jan 13, 2032 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/12292
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
In a method for producing hot-rolled sections of steel with a rectangular or square cross-section, a substantially round pipe blank produced seamlessly by hot rolling or cold finished and welded and having a defined nominal outside diameter is initially produced and then formed at a forming temperature into a hollow section having the required cross-section, with visible edges C1 and C2 of the hollow section having a value ≦1.5×t (t=wall thickness). The pipe blank has a nominal outer diameter determined from a reduction ratio of the pipe blank to be achieved and the hollow section dimensions to be achieved, wherein the reduction ration lies within a range of −2% to −13% and is determined according to the following formula:Reduction ratio R[%]=[(2×(H+B))−π×D]×100%/[2×(H+B)].
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.