Laser/arc hybrid welding method and method for producing welded member using same

US9061374B2 · kind B2 · utility

1Cited by
2References
6Claims
0Family size

Assignees

Inventors

Key dates

Filing dateMar 4, 2011
Grant dateJun 23, 2015
Priority date
Expiry dateJul 27, 2031

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB23K2103/50
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

Disclosed are: a welding method capable of increasing the welding speed up to approximately 20 m/min., yet capable of producing good bead configurations and preventing welding defects such as blowholes; and a method of producing a welded member using the welding method. Specifically disclosed is a laser/arc hybrid welding method for butt-welding flat plates of stainless steel, titanium, or titanium alloy, or butt-welding both ends of a strip-shaped plate of stainless steel, titanium, or titanium alloy which has been formed into a tubular shape, wherein in the butt welding, the laser beam irradiation and the arc discharge trace the same welding line in such a manner that laser welding is followed by TIG arc welding.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.