Abstract

A lithium aluminosilicate glass and a method for producing such lithium aluminosilicate glass are provided. The glass has a composition, in mol %, of: SiO2 60-70; Al2O3 10-13; B2O3 0.0-0.9; Li2O 9.6-11.6; Na2O 8.2-less than 10; K2O 0.0-0.7; MgO 0.0-0.2; CaO 0.2-2.3; ZnO 0.0-0.4; ZrO2 1.3-2.6; P2O5 0.0-0.5; Fe2O3 0.003-0.100; SnO2 0.0-0.3; and CeO2 0.004-0.200. Further, the composition complies with the following relations and conditions: (Li2O+Al2O3)/(Na2O+K2O) greater than 2; Li2O/(Li2O+Na2O+K2O) greater than 0.47 and less than 0.70; CaO+Fe2O3+ZnO+P2O5+B2O3+CeO2 greater that 0.8 and less than 3, where at least four out of the six oxides are included. The glass exhibits a modulus of elasticity of at least 82 GPa and has a glass transition point below 540° C. and/or a working point below 1150° C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.