Method of curing thermoplastic polymer for shape memory material
US9120898B2 · kind B2 · utility
5Cited by
47References
17Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 8, 2011 |
| Grant date | Sep 1, 2015 |
| Priority date | — |
| Expiry date | Oct 29, 2032 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L81/04
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method of preparing a cured thermoplastic material includes curing a thermoplastic polymer having a thermal decomposition temperature greater than or equal to about 200° C., at a temperature of about 200° C. to about 400° C., for a total time of less than or equal to 200 hours. A method of making a shape memory material also includes curing a thermoplastic polymer to prepare a cured thermoplastic material.