Method for preparing a thermoplastic polyurethane of improved yellowness index, and optical articles made therefrom
US9169373B2 · kind B2 · utility
1Cited by
5References
11Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | May 27, 2010 |
| Grant date | Oct 27, 2015 |
| Priority date | — |
| Expiry date | Aug 2, 2030 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G18/838
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Method for converting a composition into thermoplastic polyurethane, said composition comprising polyurethane resin, said method comprising the steps of combining the composition with a chemical compound, and converting said mixture into thermoplastic polyurethane, characterized in that said chemical compound is 1,4-Di(2,6-dibromo-4-methylphenylamino)anthracene-9,10-dione. Article obtained according to this method.