Polyethylene having faster crystallization rate and improved environmental stress cracking resistance

US9187627B2 · kind B2 · utility

16Cited by
14References
10Claims
0Family size

Assignee

Inventor

Key dates

Filing dateOct 23, 2008
Grant dateNov 17, 2015
Priority date
Expiry dateJan 10, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L2205/24
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Disclosed is a polyethylene composition having faster crystallization rate and improved environmental stress cracking resistance. The polyethylene composition comprises a multimodal polyethylene and a nucleating agent. The multimodal polyethylene comprises from 25 to 50 wt % of a low molecular weight ethylene homopolymer component, from 25 to 50 wt % of a medium molecular weight ethylene copolymer component and from 25 to 50 wt % of a high molecular weight ethylene copolymer component. The polyethylene composition has an environmental stress cracking resistance (ASTM D1693, Condition B in 100% Igepal) greater than or equal to 40 days and a crystallization half time less than or equal to 70% of the crystallization half time of the multimodal polyethylene without nucleating agent.