Patent · US Active

Method for preparing amorphous iron oxide hydroxide

US9205407B2 · kind B2 · utility

0Cited by
0References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 21, 2012
Grant dateDec 8, 2015
Priority date
Expiry dateMay 21, 2032

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/80
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for preparing amorphous iron oxide hydroxide, comprising following steps: (1) preparing a ferrous salt solution with solid soluble ferrous salt; (2) preparing a hydroxide solution; (3) mixing said hydroxide solution and said ferrous salt solution in a co-current manner for reaction at an alkali ratio of 0.6˜0.8 and a reaction temperature not exceeding 30° C.; (4) after the reaction in step (3) is finished, yielding a first mixture, then charging said first mixture with a gas containing oxygen for oxidation, and controlling the first mixture at a pH value of 6˜8 until the oxidation is finished to yield a second mixture; and (5) filtering, washing with water and drying said second mixture obtained in step (4) to yield the amorphous iron oxide hydroxide.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.