Cast CrMoV steel alloys and the method of formation and use in turbines thereof

US9206704B2 · kind B2 · utility

0Cited by
3References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 11, 2013
Grant dateDec 8, 2015
Priority date
Expiry dateJan 25, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A cast alloy is generally provided, along with methods of forming the cast alloy and components constructed from the cast alloy (e.g., stationary components of a turbine). The cast alloy can include, by weight, 0.12% to 0.20% carbon, 0.50% to 0.90% manganese, 0.25% to 0.60% silicon, 0.10% to 0.50% nickel, 1.15% to 1.50% chromium, 0.90% to 1.50% molybdenum, 0.70% to 0.80% vanadium, 0.0075% to 0.060% titanium, 0.008% to 0.012% boron, the balance iron, optionally low levels of other alloying constituents, and incidental impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.