Abstract
In a process for producing high molecular weight polyethylene, ethylene is contacted with a slurry of a catalyst composition comprising a Group 4 metal complex of a phenolate ether ligand under polymerization conditions comprising a temperature of about 20° C. to less than 90° C. and a pressure of about 4 bar to about 40 bar.