Active material for nonaqueous secondary battery and method for producing same
US9240593B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 21, 2006 |
| Grant date | Jan 19, 2016 |
| Priority date | — |
| Expiry date | Oct 12, 2029 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
There is provided a method for producing an active material for a nonaqueous secondary battery, including firing an adherend in which a compound containing an element A (at least one element selected from among B, Al, Ga, In, Si, Ge, Sn, Mg and transition metal elements) is adhered to a particle surface of a material capable of being doped and dedoped with lithium ions, in a water-containing atmosphere so that weight increasing rate of the adherend is in a range of 0.1% by weight or more and 5.0% by weight or less, and firing the adherend.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.