Cr-containing austenitic alloy tube and method for producing the same

US9255319B2 · kind B2 · utility

2Cited by
1References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 12, 2011
Grant dateFeb 9, 2016
Priority date
Expiry dateJan 25, 2032

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E30/30
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

There is provided a Cr-containing austenitic alloy tube, wherein a chromium oxide film with a thickness of 0.05 to 1.5 μm having the relationship defined by Formula (i) is formed on the inner surface of the tube, wherein the average concentration of C in the depth range of 5 to 10 μm from the inner surface is lower than the concentration of C in a base metal;0.4≦δ1/δ2≦2.5  (i)wherein δ1 and δ2 are thicknesses (μm) of the chromium oxide film at both ends of tube, respectively.