Micropowder and molding containing a zeolitic material containing Ti and Zn
US9296714B2 · kind B2 · utility
0Cited by
6References
37Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Feb 5, 2013 |
| Grant date | Mar 29, 2016 |
| Priority date | — |
| Expiry date | Feb 5, 2033 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB01J2235/30
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.