Aqueous dispersion liquid and coating material, film, and product using the same

US9321034B2 · kind B2 · utility

2Cited by
6References
13Claims
0Family size

Assignees

Inventors

Key dates

Filing dateMar 6, 2014
Grant dateApr 26, 2016
Priority date
Expiry dateMar 6, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08K3/22
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

In one embodiment, an aqueous dispersion liquid contains at least one particles selected from tungsten oxide particles and tungsten oxide composite particles. A mean primary particle diameter (D50) of the particles is in the range of 1 nm to 400 nm. In the aqueous dispersion liquid, concentration of the particles is in the range of 0.1 mass % to 40 mass %, and pH is in the range of 1.5 to 6.5. The aqueous dispersion liquid excels in dispersibility of particles and capable of maintaining good liquidity for a long period.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.