Abstract
A refractory ceramic batch with the composition of 75 to 98% by weight of at least one basic base material from the group having sintered magnesia and fused magnesia, 2 to 25% by weight. of at least one granular aggregate from the group having silicon carbide, silicon nitride, silicon oxycarbide, silicon oxycarbonitride, and a maximum 5% by weight of other constituents.