Methods for forming delamination resistant glass containers

US9346707B2 · kind B2 · utility

19Cited by
136References
29Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 25, 2013
Grant dateMay 24, 2016
Priority date
Expiry dateFeb 21, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/315
  • WIPO fieldHandling
  • WIPO sectorMechanical engineering

Abstract

In one embodiment, a method of forming a glass container may include forming a glass container comprising a sidewall at least partially enclosing an interior volume. At least a portion of the interior surface of the sidewall may have an interior surface layer with a persistent layer heterogeneity relative to a midpoint of the sidewall. The interior surface layer of the glass container may be removed from the interior surface of the sidewall such that a modified interior surface of the sidewall has an interior region extending from about 10 nm below the modified interior surface into a thickness of the sidewall. The interior region may have a persistent layer homogeneity relative to the midpoint of the sidewall such that the modified interior surface is resistant to delamination.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.