Method of synthesis of a composition containing at least one internal dehydration product of a hydrogenated sugar by heterogeneous catalysis
US9346819B2 · kind B2 · utility
0Cited by
2References
20Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Aug 7, 2013 |
| Grant date | May 24, 2016 |
| Priority date | — |
| Expiry date | Aug 7, 2033 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC07D493/04
- WIPO fieldOrganic fine chemistry
- WIPO sectorChemistry
Abstract
A simple, low cost, environmentally friendly and sustainable process for the production of internal dehydration products of hydrogenated sugar, implementing trivalent metal phosphate (metal (III) phosphates) as catalysts during the dehydratation step.