Fin stock material
US9377249B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jun 8, 2015 |
| Grant date | Jun 28, 2016 |
| Priority date | — |
| Expiry date | Jun 8, 2035 |
Classification
- Technology area (CPC F)Mechanical Engineering; Lighting; Heating
- CPC primaryF28F2275/04
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A fin stock material from an 3xxx-series aluminum alloy and including at least 0.5% to 2.0% Mn, and furthermore a purposive addition of one or more wetting elements selected from the group of: Bi 0.03% to 0.5%, Pb 0.03% to 0.5%, Sb 0.03% to 0.5%, Li 0.03% to 0.5%, Se 0.03% to 0.5%, Y 0.03% to 0.05%, Th 0.03% to 0.05%, and the sum of these elements being 0.5% or less, with the remainder including aluminum and tolerable impurities. Also provided is a method for manufacturing a heat exchanger assembly incorporating such a fin stock material.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.