Glass ceramics having low rhodium levels
US9403715B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 23, 2014 |
| Grant date | Aug 2, 2016 |
| Priority date | — |
| Expiry date | Sep 2, 2034 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/315
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A glass ceramic precursor glass and a glass ceramic having low levels of rhodium and a method of controlling the amount of rhodium in such glasses and glass ceramics. The precursor glass and glass ceramic contain from about 1 ppm to about 10 ppm and, in certain embodiments, from about 1 ppm to about 6 ppm rhodium. The method of controlling of reducing rhodium dissolution from a rhodium-containing material such as, for example, an alloy into a glass melt comprises controlling and/or lowering the partial pressure of oxygen at the rhodium-containing vessel/glass interface by imposing a high humidity condition around the external (non-glass-contact) surface of the rhodium-containing material. The lower concentration of rhodium minimizes its coloring effect on the white color of the glass ceramic.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.